A brand choosing a textured face is usually shown three routes. Those are raw T700 carbon with a peel-ply finish, silicon carbide grit, and ceramic sand mixed into the resin. Each supplier can show a paddle that grips the ball on day one. Far fewer can show what the same face measures after a controlled wear run. Fewer still can show the spin number and the roughness number taken on the same samples.

That gap matters because height and spin follow separate paths as a face wears. A face can hold most of its surface height and still give up spin. A face that looks worn can keep more grip than expected. This article puts the three routes side by side using the figures we can verify. It then explains what our own test bench measures. It also covers how the tooling behind a custom face is protected.

The last section covers a separate question that buyers raise once the technical choice is made. A texture that works is worth little if another brand can order the same shape and surface a month later. The mold agreement and the patent position decide whether that can happen.

The Three Routes Differ in How the Grit Is Held

The first route is a raw T700 face with a peel-ply texture. A cloth is pressed against the resin during curing and peeled away afterward, leaving the cloth pattern in the surface. The texture height is limited by the weave and the resin used in the layup. That puts its friction ceiling below a grit-loaded face.

The second route is silicon carbide. The hard particles can be embedded in the weave, layered on the face, or mixed into the resin before pressing. Those are different builds, and they wear in different ways. A supplier quoting “SiC” without saying which of the three it uses has not given you a specification.

The third route is ceramic sand infused into the resin before layup. We mix 80 or 100 mesh ceramic grit into the resin. We coat the face plies and cure the stack in a heated mold. Each grain sits in cured resin with only its tip exposed. The grit is held by the whole face rather than by a surface film.

What the Published Numbers Actually Say

Public figures for these routes come from different rigs, so they cannot be dropped into one ranking. The route-by-route breakdown in how the three grit routes compare in a wear test sets out what each finish changes. The table below separates two kinds of figures. One is what a supplier reports about its own SiC and spray-grit processes. The other is what we measured on our own faces. The conditions are written beside each figure because a retention percentage has no meaning without its test length.

Route

Roughness reported

Friction / spin reported

Wear figure and its basis

Peel-ply raw carbon

Ra 1.8–3.2 µm, Rz 8–15 µm

COF 0.12–0.16; 1,800–2,100 RPM

70–80% retention at 50 h, supplier report

Silicon carbide, resin-integrated

Ra 2.0–4.6 µm, Rz 11–22 µm

COF 0.14–0.19; 1,900–2,300 RPM

85–90% at 60 h, supplier’s own test

Sprayed grit coating

Ra 3.0–8.0 µm, Rz 16–26 µm

COF 0.14–0.19; 1,950–2,200 RPM

40–55% at 50 h; enhanced process 50–75%

Ceramic sand infused, our run

Read on our profilometer per batch

1,668.83 RPM before, 1,621.99 after

47 RPM lost over 100 cannon hits at 90 km/h

The first three rows come from a public supplier comparison read on 27 November 2026. They describe that supplier’s own processes rather than an independent lab. We include them because they show the range of claims a buyer will meet, not because we can confirm each number. The fourth row is our own test, and the conditions are fixed. We used one paddle style, one ball speed, six readings before and six after.

The spray-grit row is where the phrase “grit falls off” has a clear meaning. A particle sitting in a surface film can be knocked out of that film, and the bare spot underneath reads smooth. The SiC rows describe a different failure mode. Those particles are held in cured resin. The more useful question is how the bond and the exposed tip wear under repeated impact. It is not a question of whether the whole grain leaves the face all at once during play.

Roughness Retention and Spin Retention Are Not the Same Test

A profilometer measures the height difference between the peaks and valleys on a face. A ball cannon measures what the face does to a ball. Both are legitimate, and they answer different questions for a buyer deciding which surface to specify.

A face can keep most of its Rz and still lose spin. That happens when the peak shape rounds over under repeated ball impact. It also happens when the resin between the peaks polishes smooth. The ball then touches a broader, flatter surface. The height reading stays close to its starting value while the friction at contact drops. A retention percentage from a profilometer cannot tell you how much spin a player loses.

Our own run measured spin directly and published the raw spread alongside the mean. Six shots before the wear run ranged from 1,548 to 1,793 RPM. The six after the run spread across a similar band. The 47 RPM mean loss is smaller than the scatter inside a single set. One shot before and one shot after cannot support a claim. The control face in the same run lost about 100 RPM, putting our loss at roughly 2.1 times smaller.

That result describes one structure in one test, and we do not present it as a benchmark for the category. Our cannon protocol has only been run against our own faces and a sprayed control. The public retention figures belong to their authors and stay separate from our run. A buyer who wants a head-to-head number should ask each supplier for spin measured before and after the same protocol.

Our Bench Measures the Face and the Build Around It

We hold twelve test machines in our own plant, listed in an equipment record dated 10 November 2026. Three of them do most of the work in a grit wear study. A KEYENCE 3D profilometer maps the face in three dimensions. A surface roughness tester reads Ra and Rz line by line. A gloss meter records how much light the face reflects, which rises as a textured surface polishes smooth.

A ball cannon fires at a fixed speed and angle, and a COR tester records rebound and spin off the face. Repeated-hit and impact fatigue testers run the same spot again and again to find a drop in the reading. An X-ray unit looks inside the finished paddle for voids and layers coming apart. That matters when a grit change also changes the press cycle. The remaining machines cover peel strength, swing weight, twist weight and the sound a paddle makes at contact.

What a buyer needs to know

Machine that reads it

What we hand over

Face height and profile

KEYENCE 3D profilometer, surface roughness tester

Roughness readings with the test date

Spin before and after wear

Ball cannon, COR tester

Six readings on each side of the run

Surface polishing

Gloss meter

One gloss number beside the roughness number

Bond failure under load

Universal testing machine, impact fatigue tester

Hit count and reading before and after

Internal voids after a press change

X-ray CT inspection

Image of the scanned paddle

The equipment list matters less than the protocol written around it. The full instrument list in what our test bench can measure shows the readings each machine produces. We fix the ball speed at 90 km/h and use six shots on each side of the run. We take a cut sample from the batch instead of a hand-finished display paddle. A machine count on a factory tour tells you what could be measured. The dated readings tell you what was measured.

USAP Sets a Ceiling, Not a Ranking

Certification limits apply to the finished model, whatever route produced its texture. USAP sets average Rz at or below 30 µm and Rt at or below 40 µm. It also sets a friction limit of 0.1875 and a gloss limit of 80 GU. The dual-camera spin test added for new submissions in October 2026 measures the finished paddle rather than the grit powder.

That ceiling changes how a face should be specified. A route that starts near the roughness limit has little room left. A new sample that reads high can cross the line on another batch. A face that starts lower keeps more room for batch variation. It may give a player less bite on day one. Neither direction is automatically better, because the limit belongs to the model and not to the process name.

The public figures in the comparison table include routes with a reported Rz up to 26 µm. Their reported COF reaches 0.19. Those numbers sit close to the certification limits. That is a reason to ask for readings on the exact sample being submitted. A supplier who quotes a category average cannot tell you whether your model will pass. Our own pre-check reads the sample before the brand files it. Approval still belongs to the brand that submits the model.

The 55+ Patents Cover Process as Well as Structure

A texture choice stops being a technical question when a brand finds the same face on a competitor’s paddle. That is where the patent position and the mold agreement become part of the specification. Our public company record lists more than 55 patents in racket technology, including the ceramic sand infused surface process. The engineering team is led by a professor with twenty years in composites and works with a university composite research center.

Patents cover what the claim actually describes, rather than every feature on a finished paddle. A brand should ask which patent numbers relate to the surface it is buying. It should also ask which countries those patents are in force in. A patent count says little about one specific paddle design and the claims it touches. We do not offer a legal opinion on a competitor’s product or on any claim they publish. We can name the patents behind our own process and put the relevant numbers in the development file.

The private mold question is separate from the patent position. A mold cut for one brand’s shape can be stored under that brand’s name. The agreement should say who holds the tooling and who may use it. Four terms need settling before the first sample. They are plate ownership, tool custody, replacement cost, and whether the cavity can run another brand’s order. Those terms belong in writing before the first sample is pressed.

A supplier that shares a design across several brands will answer that last question differently from one that dedicates a plate. The tooling terms in how a private mold stays yours show how a dedicated plate is handled. Neither answer is wrong on its own, but the brand needs to know which one it is buying. A written clause that says the shape and surface are exclusive is worth more than a verbal promise made during sampling. We can show the tooling record and the patent list once a drawing and a target spec are in hand.

What to Ask Before You Approve a Surface

A surface approval should end with a short set of documents rather than a favorable first impression. A useful approval file holds the roughness and gloss readings on the sample. Those readings need a date and a named instrument. The same file should hold spin measured before and after a wear run. It should show how many readings were taken and how wide the scatter runs. The file should also name the exact grit route quoted in the offer. The word “SiC” on its own does not name the particular build being offered for your line.

The tooling and patent terms belong in the same meeting. The answer should state who owns the plate and where it is stored. It should name the patents covering the surface being supplied. A supplier that can answer these questions with dated records has shown how the face is controlled. A supplier that answers with adjectives has given you a starting point for a conversation, not a specification.

The table and the figures in this guide give you a way to read the answers. None of them replaces a test run on your own sample. The face you approve is the one that has to pass and to stay exclusive.

FAQ

Which route keeps spin longest? The answer depends on how the grit is held and how the test is run. Our ceramic sand face lost 47 RPM across 100 cannon hits at 90 km/h. A sprayed control face lost about 100 RPM in the same run. Public supplier figures put resin-integrated SiC at 85–90 percent texture retention after 60 hours. Those two formats measure different things, and no shared protocol has been published across all three routes.

Does a silicon carbide face shed grit? A sprayed coating can lose whole particles when a grain is knocked out of the surface film. A resin-integrated SiC grain is held through the cured resin, so it wears down rather than leaving all at once. The supplier comparison we cite reports stronger retention for resin-integrated SiC than for spray grit. That report is a supplier’s own test, read on 27 November 2026, and we have not repeated it on our bench.

What does the 2.1× figure compare? It compares spin loss on our ceramic sand face with a sprayed control face. Both were measured in the same cannon run. Our face lost 47 RPM and the control lost about 100 RPM over 100 hits at 90 km/h. It is not a comparison against silicon carbide, and it is not an industry benchmark.

Do the roughness limits apply differently to each route? No. USAP applies average Rz ≤ 30 µm, Rt ≤ 40 µm, COF ≤ 0.1875 and gloss ≤ 80 GU to the finished model. The route used to build the face does not change those limits. A face that starts close to the ceiling has less room for batch variation.

Can a brand own the mold used for its face? That is a term of the agreement rather than a property of the surface. A private plate can be held in the brand’s name, with custody and replacement terms written into the contract. The agreement should name who may run the same cavity, in writing before the sample is approved.

Do the 55+ patents cover the ceramic sand process? Our public company record lists more than 55 patents in racket technology, including the ceramic sand infused surface process. A buyer should review the patent numbers and the countries where they are in force. A patent count is not a legal opinion about a competitor’s product.